Open today by appointment

en

Reclaimed wood beams

Reclaimed oak beams

Reclaimed pine beams

Reclaimed elm beams

Reclaimed oak joists

Reclaimed purlins

Reclaimed mooring posts

Reclaimed american pine beams

Reclaimed wooden pedestal

Air dried oak beams

Oak beams air dried

Oak purlins air dried

Long oak planks

Long oak beams

Oak Rails Air Dry

Architectural beam selections

Antique french oak beams

18th century oak beams

Majestic antique oak beams

Silver seasoned oak beams

19th century elm beams

Oak table

Reclaimed oak table

Wagon plank table

Oak monastery table

Round Oak Table

Oak tree trunk table

Reclaimed oak outdoor table

Reclaimed wood planks

Oak Reims planks

Reclaimed pine planks

Oak track boards

Reclaimed oak planks

Reclaimed oak wine press boards

Reclaimed Oak Haystack Shelves

Barnwood Planks

Reclaimed harbor shelves

Live edge oak planks

French oak planks

Reclaimed wagon boards

Oak wagonboards brushed

Reclaimed wagonboards planed

Reclaimed hardwood wagonboards

Reclaimed pine and spruce wagon boards

Wood flooring

Reclaimed oak floor

French oak floor

Reclaimed oregon pine floor

Reclaimed pine floor

Reclaimed wooden wall cladding

Reclaimed oak wall cladding

Barnwood wall covering

Wood ceiling

Reclaimed oak roof boarding

Reclaimed roof boarding boards

French oak roof boarding

Wood cladding

Oak cladding

Architectural collection

Oak planks – planed and kiln-dried

18 century oak bench

Long reclaimed oak table

Reclaimed oak door

Solid reclaimed oak coffee table

menu

Open today by appointment

+31(0) 488 455 025

en
stories

How thick should old oak planks be for a floor?

As a rule of thumb, an antique oak floor should have a thickness of at least 20 mm after finishing. In practice, reclaimed oak floorboards typically range between 22 and 35 mm, depending on the application, the subfloor, and whether underfloor heating is present. The sections below cover the factors that determine the right choice.

Which thickness is suitable for which use?

The right thickness for a wooden floor depends on the application. For living spaces on a stable subfloor, 20 to 25 mm is generally sufficient. For heavier use, such as commercial spaces or floors on joists, 28 to 40 mm is a more logical choice. The desired aesthetic and the structural situation together determine what works best.

A thin board of 20 mm produces a cleaner, more modern result and is lighter in weight. A thicker board of 30 mm or more has more character, greater surface relief, and can be refinished more often over its lifetime. For projects where the wood also plays a structural role — for example, a floor on wooden beams without an additional load-bearing structure — sufficient thickness is not a choice but a necessity.

What is the minimum thickness for an antique oak floor?

The minimum thickness for an antique oak floor after finishing is 18 mm, but 20 mm is in practice the lower limit that most installers adhere to. Below that threshold, the risk of movement, cracking, or insufficient rigidity increases — particularly with reclaimed wood that already has its own drying history.

Antique oak is naturally more stable than new wood, having already moved and settled over decades or centuries. Even so, a minimum material thickness is still required for the wood to perform properly. When boards are sawn from old beams, it is also wise to allow some margin for finishing: planing, sanding, or brushing always removes a few millimeters.

How does underfloor heating affect the required thickness?

With underfloor heating, the maximum recommended thickness for solid wooden floorboards is 22 mm. Thicker wood insulates more and impedes heat transfer, making the system less efficient and exposing the boards to greater temperature differences between the top and bottom. For reclaimed oak with underfloor heating, a thickness of 18 to 22 mm is a popular choice.

Oak responds to heat and moisture fluctuations by moving slightly. With underfloor heating, those fluctuations are greater than with an unheated floor, because the system warms the boards from below while the top surface remains at room temperature. Antique oak has an advantage due to its long drying time: the material has already stabilized and reacts less dramatically than freshly sawn wood. Even so, it remains advisable not to choose boards that are too thick, and to start the heating system gradually after installation.

What is the difference between sawn and planed thickness?

The sawn thickness is the measurement directly after sawing; the planed thickness is what remains after the boards have been surface-planed or milled. The difference is typically 2 to 4 mm per side that is processed. A board sawn to 28 mm may end up at 22 to 24 mm after planing.

This distinction matters when ordering old oak boards for a flooring project. The measurement listed in the specifications is not always the final measurement after finishing. With reclaimed wood, this is an additional consideration, since the boards are sometimes not completely flat and need to be lightly processed on both sides to achieve an even result. When ordering, always ask for the net measurement after finishing, not just the rough measurement.

When should you choose thicker boards over thinner ones?

Thicker boards are a logical choice when the floor rests on joists, when heavy traffic is expected, or when the wood needs to be refinished multiple times in the future. Aesthetics can also tip the balance in favor of a thicker board: deeper grain, more surface relief, greater mass.

The choice depends on several factors at once. An architect working on a listed building will weigh things differently than a contractor finishing a new home. Relevant considerations include:

  1. Structure: Is the floor on concrete or on wooden beams? On beams, greater thickness is needed for rigidity.
  2. Lifespan and maintenance: A thicker board can be sanded and refinished more often.
  3. Underfloor heating: Is it present? If so, thinner is often better for heat transfer.
  4. Build-up height: How much space is available above the structural floor?
  5. Appearance: A thicker board looks more robust and accentuates the character of old wood.

For many residential projects, a thickness of 25 to 30 mm is a popular middle ground: strong enough, easy to finish, and compatible with most subfloors.

How do you measure the usable thickness of reclaimed boards?

The usable thickness of reclaimed boards is measured at the thinnest point of the board, after removing dirt, nails, and loose fibers. That is the measurement that determines what remains after finishing. Use a caliper or depth gauge at multiple points along the length of the board.

Reclaimed boards are rarely completely uniform in thickness. Old sawmills worked with less precision than modern machinery, and decades of use leave their mark. A variation of 2 to 4 mm along the length of a board is normal. When measuring for a project, it is advisable to work from the minimum thickness, not the average.

Would you like to assess the boards in person before making a decision? That is possible. Visit the timber yard in Doorwerth and view the stock on site. That way you can see exactly what is available and what the material will yield after finishing. For inspiration on how other projects have been realized, you are also welcome to browse the projects page.

How Frank Pouwer helps you find the right thickness for your floor

The question of the right thickness is rarely separate from the rest of the project. Structure, subfloor, heating, appearance, and available material all play a role. We think along with you, from the initial material selection through to custom sawing.